LLlx0105 发表于 2018-2-6 11:50:52

Solder paste 化金面积不准确

化金面积调试:好像不准skill导出如下图

SOLDER PASTE PADS FOR SIDE A:-----------------------------Count   Size-----   ----196   16cir158   20x25   64   11x64   32   12x35   26   32x35   20   50x50   10   31x47    8   63x79    825x80    8   94x94    6   47x71    6   55x87    5   27x39    4   76x88    4   40cir    3   40x55    3   67x87    3   106x165    2   71x224    2   35x83    2   63x102    2   100x100    1   87x157    1   100x120    1   134x134Solder Paste Area For Side A: 673396 sq. milsSolder Paste Pad Count For Side A: 575SOLDER PASTE PADS FOR SIDE B:-----------------------------Count   Size-----   ----130   20x25   54   16x63   26   32x35   16   50x50   12   134x252    8   24x114    6   63x102    4   40cir    3   106x165    2   55x87Solder Paste Area For Side B: 719992 sq. milsSolder Paste Pad Count For Side B: 261结论:A: 673396 sq. mils+ B:719992 sq. mils=top面+bottom面=1393388 sq. mils化金面积=soldermask的总面积除以pcb面积即:Pcb的面积:3149.6*3937.0【mil×mil】1393388/3149.6/3937=11%而CAM350算得为58%


bingshuihuo 发表于 2018-2-28 13:57:48

这个到底怎么计算?
页: [1]
查看完整版本: Solder paste 化金面积不准确